Skip navigation
Home
Browse
Communities
& Collections
Browse Items by:
Issue Date
Author
Title
Subject
Item Type
Advanced Search
Help
About DSpace
Sign on to:
My DSpace
Receive email
updates
Edit Profile
Saved Searches
Favorites
Repository of UOI "Olympias"
Repository of OAI
Saved Searches
Save this search
Go!
Discover
Author
2
Karantzalis, A. E.
1
Arni, Z.
1
Dracopoulos, V.
1
Georgatis, E.
1
Tsirka, K.
Subject
2
crystal growth
2
growth morphologies
2
kinetics
2
mc carbide morphologies
1
crystals
1
intermetallic matrix composites
1
intermetallics
1
laser
1
matrix composites
1
ni-al intermetallic
.
next >
Date
1
2012
1
2011
Search
Search:
All of DSpace
ΑΠΟΘΕΤΗΡΙΟ "ΟΛΥΜΠΙΑΣ"
Σχολή Θετικών Επιστημών
Τμήμα Μηχανικών Επιστήμης Υλικών
Άρθρα σε επιστημονικά περιοδικά ( Ανοικτά)
for
Search only items with full text availability
Current filters:
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
Clear current filters
or
Add more filters
Title
Author
Subject
Date Issued
Item Type
Date
Has File(s)
???jsp.search.filter.original_bundle_filenames???
???jsp.search.filter.original_bundle_descriptions???
Equals
Contains
ID
Not Equals
Not Contains
Not ID
View Option
Results/Page
5
10
15
20
25
30
35
40
45
50
55
60
65
70
75
80
85
90
95
100
Sort items by
Relevance
Title
Issue Date
In order
Ascending
Descending
Authors/record
All
1
5
10
15
20
25
30
35
40
45
50
Results 1-2 of 2 (Search time: 0.002 seconds).
previous
1
next
Solidification observations and sliding wear behavior of vacuum arc melting processed Ni-Al-TiC composites (Journal article)
Solidification observations of vacuum arc melting processed Fe-Al-TiC composites: TiC precipitation mechanisms (Journal article)