dc.contributor.authorMei, S.en
dc.contributor.authorYang, J.en
dc.contributor.authorXu, X.en
dc.contributor.authorQuaresma, S.en
dc.contributor.authorAgathopoulos, S.en
dc.contributor.authorFerreira, J. M. F.en
dc.date.accessioned2015-11-24T17:32:09Z-
dc.date.available2015-11-24T17:32:09Z-
dc.identifier.issn0955-2219-
dc.identifier.urihttps://olympias.lib.uoi.gr/jspui/handle/123456789/13679-
dc.rightsDefault Licence-
dc.subjecttape castingen
dc.subjectsolids loadingen
dc.subjectrheological behavioursen
dc.subjectcordieriteen
dc.subjectbinderen
dc.subjectglass-ceramicsen
dc.subjectrheological characterizationen
dc.subjectmechanical-propertiesen
dc.subjectsilicon-nitrideen
dc.subjectgreen tapesen
dc.subjectaluminaen
dc.subjectslurriesen
dc.subjectpackageen
dc.titleAqueous tape casting processing of low dielectric constant cordierite-based glass-ceramics - selection of binderen
heal.typejournalArticle-
heal.type.enJournal articleen
heal.type.elΆρθρο Περιοδικούel
heal.identifier.primaryDOI 10.1016/j.jeurceramsoc.2004.10.020-
heal.identifier.secondary<Go to ISI>://000233581400008-
heal.identifier.secondaryhttp://ac.els-cdn.com/S0955221904004881/1-s2.0-S0955221904004881-main.pdf?_tid=36af5710047e8f471963b7f9de910674&acdnat=1339492650_f839269706bc9b0174f2e1a1f83e64e2-
heal.languageen-
heal.accesscampus-
heal.recordProviderΠανεπιστήμιο Ιωαννίνων. Σχολή Θετικών Επιστημών. Τμήμα Μηχανικών Επιστήμης Υλικώνel
heal.publicationDate2006-
heal.abstractIn this paper, four different binders were investigated in the process of aqueous tape casting of cordierite-based glass-ceramics and their effects on the rheological behaviour of the suspensions and on the microstructures of the green tapes were compared. Meanwhile, a good compatibility between the dispersant and binder was found to be a predominant factor to obtain an optimised cordierite glass-ceramic tape. The microstructure of the green tape was observed by SEM and the weight loss during binder burn out process was determined by DTA/TG. The dielectric constant and dielectric loss of the sintered tapes (at 1150 degrees C for 2 h) was also measured. (c) 2004 Elsevier Ltd. All rights reserved.en
heal.publisherElsevieren
heal.journalNameJournal of the European Ceramic Societyen
heal.journalTypepeer reviewed-
heal.fullTextAvailabilityTRUE-
Appears in Collections:Άρθρα σε επιστημονικά περιοδικά ( Ανοικτά)

Files in This Item:
File Description SizeFormat 
Mei-2006-Aqueous tape casting.pdf817.59 kBAdobe PDFView/Open    Request a copy


This item is licensed under a Creative Commons License Creative Commons